Phosphate combined alumina brick

Product Description

Phosphate combined alumina brick

Item

Unit

Phosphate bricks  P

Abrasion resistant brick PA

Ⅰ

Ⅱ

Ⅰ

Ⅱ

Al2O3 ≥

%

75

77

Fe2O3 ≤

%

3.2

3.2

CaO

%

0.6

0.6

Bulk density ≥

g/cm3

2.70

2.65

2.75

2.70

Cold crushing strength ≥

Mpa

70

60

75

65

Refractoriness under load ≥

℃

1350

1300

1300

1250

Thermal shock resistance 1100℃ water cooling ≥

times

10

10

10

10


Product Inquiry